RXD Polyurethane Rubber U75 A+B is a professional two-component polyurethane elastomeric resin, designed for applications requiring high mechanical strength, excellent wear resistance, and greater hardness than U45. With a hardness of 75 Shore A, it is an ideal choice for industrial molds, rollers, coatings, protective parts, and high-stress applications.
Packaging: 2kg (1kg Part A + 1kg Part B)
Ideal for:
- Artificial stone molds
- Cement decorations
- Industrial molds
- Polyurethane rollers
- Protective coatings
- Durable parts
- Prototype tooling
- High wear applications
Advantages:
- High hardness (75 Shore A)
- Excellent wear resistance
- Very high tear strength
- High mechanical strength
- Low shrinkage
- Mixing ratio 1:1
- High dimensional stability
- Long service life
Technical specifications:
- Mixing ratio: 1:1
- Color: Part A: Light yellow | Part B: Transparent
- Hardness: 75 Shore A
- Viscosity: Part A: 750 ±200 mPa·s | Part B: 1600 ±200 mPa·s
- Working time: 30–40 minutes
- Full curing: 16–24 hours
- Tear strength: 28 kN/m
- Tensile strength: 10 MPa
- Elongation: 350–450%
- Resilience: 50%
- Density: 1.10 g/cm³
- Linear shrinkage: 0.1%
Instructions for use:
- Mix equal amounts of Part A and Part B.
- Stir well until the mixture is homogeneous.
- Pour the material into the mold or desired surface.
- Allow to cure at room temperature for 16–24 hours.
- After full curing, it achieves excellent mechanical strength and long service life.
Manufacturer
OEM- Product Number
- 13691
- Type
- Silicone Calypso
- Construction Material [Pharmaceutical]
- -
- Colour
- Yellow
Important information
Specifications are collected from official manufacturer websites. Please verify the specifications before proceeding with your final purchase. If you notice any problem you can report it here.